Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources PPX-FR2-[color]-EN Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -30.0 °C |
2.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-GP1 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -30.0 °C |
2.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-GP1-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Extrusion Notes: All physical, mechanical and thermal testing conduc.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -30.0 °C |
2.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-GP2 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 250F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -30.0 °C |
2.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-GP3 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -30.0 °C |
2.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-GP3-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: ExtrusionNotes: All physical, mechanical and thermal testing conduct.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -30.0 °C |
2.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-GP3-WR Modified-PPO, Wear Resistant Modified-Polyphenylene Oxide, Wear Resistant, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water Absorption • Good Wear ResistanceProcess: Injection MoldingNotes: All physical, mechan.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -30.0 °C |
2.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-GP4 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources PPX-GP5 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 270F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources PPX-GP6 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 290F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature 23.0 °C |
2.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Noble Polymers Regis™ 225104 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature 23.0 °C |
2.50 ft-lb/in @Temperature 73.4 °F |
1/8" (3mm) notched bar; ASTM D256 |
Ineos L34N-00 Polypropylene Impact Copolymer Grade L34N-00 typically has a 35 melt flow rate and is a low gloss, high impact polypropylene copolymer. This material meets the requirements of the U.S. Food and Drug Administration as specified in.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -20.0 °C |
2.50 ft-lb/in @Temperature -4.00 °F |
1/8'' notched bar; ASTM D256 |
Ineos N07N-00 Polypropylene Impact Copolymer This is a medium melt flow rate, nucleated and antistatic impact copolymer polypropylene for injection molding applications that require a superior stiffness to impact balance.ApplicationsMaterials .. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.50 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF30 IM HS L 30% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI.. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.50 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 IM5 BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature 22.8 °C |
2.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced Notes: Impact Modified; Reinforced with 13% Glass Fibers; Synergistic compound exhibiting impact strength and dimensional stability Features: Good Dimensional stability; Good Processability; Heat St.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Teknor Apex Chemlon® 253 Nylon 6, Toughened Features: Medium Impact Resistance; Impact modified co-polymer grade offering strength and flexibility, especially at low temperatures Processing Method: Injection Molding Forms: PelletsInformation .. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.50 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/66 IM3 BK Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Copolymer, Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection Moldi.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature 25.0 °C |
2.50 ft-lb/in @Temperature 77.0 °F |
ASTM D256A |
Formosa Plastics Formolene® 6535N Impact Copolymer Polypropylene Impact Copolymer - Designed to Meet the Physical Requirements of Automotive Interior Trim Formolene® 6535N is an engineered, medium impact copolymer polypropylene. It was specifically developed to.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature 0.000 °C |
2.50 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
Formosa Plastics Formolene® 6613N Impact Copolymer Polypropylene Copolymer for Injection Molded Applications Requiring a Combination of High Toughness and Stiffness Formolene® 6613N is a copolymer of polypropylene designed and formulated for injection molding ap.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Clariant PA233 Nylon 6, Improved Processability, Easily Colorable, Toughened Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Clariant Renol PA233HT Nylon 6, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.50 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall 9211 Rigid PVC, Molding Georgia Gulf 9211 is a food grade vinyl compound designed to maximize clarity. It is suitable for use in a variety of food, cosmetic and personal care products.Information provided by Georgia GulfG.. |
|||
Izod Impact, Notched | >= 1.33 J/cm @Temperature -30.0 °C |
>= 2.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Buckeye Polymers BP FLEX D6017 T BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Processing Method: Injection Mold.. |
|||
Izod Impact, Notched | >= 1.33 J/cm @Temperature -20.0 °C |
>= 2.50 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Buckeye Polymers BP FLEX D7030 BLK Thermoplastic Elastomer TPV Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 6.35 mm |
2.50 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 9017 Rigid PVC, Molding Georgia Gulf 9017 is for food packaging applications requiring optimum taste and odor properties such as water and mouthwash.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporatio.. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.17 mm |
2.50 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 5006 Rigid PVC, Extrusion, Natural Georgia Gulf 5006 Natural is a rigid PVC pellet compound designed for extrusion of interior rigid PVC profiles and various contours where high gloss and ease of processing is required. Georgia Gulf.. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.17 mm |
2.50 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 5006 Rigid PVC, Extrusion, White Georgia Gulf 5006 White is a rigid PVC pellet compound designed for extrusion of rigid PVC house siding, window profiles and various contours where maximum weather resistance is required. Georgia G.. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 6.35 mm |
2.50 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 9017J Clear 06 Rigid PVC, Molding, Clear Georgia Gulf 9017J Clear 06 is for food packaging and personal care applications requiring optimum taste and odor properties. The compound contains an ultraviolet light stabilizer, which protects l.. |