Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -30.0 °C |
2.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-GP1 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -30.0 °C |
2.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-GP1-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Extrusion Notes: All physical, mechanical and thermal testing conduc.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -30.0 °C |
2.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-GP2 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 250F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -30.0 °C |
2.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-GP3 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -30.0 °C |
2.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-GP3-WR Modified-PPO, Wear Resistant Modified-Polyphenylene Oxide, Wear Resistant, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water Absorption • Good Wear ResistanceProcess: Injection MoldingNotes: All physical, mechan.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -30.0 °C |
2.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-GP4 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources PPX-GP5 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 270F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature 23.0 °C |
2.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Noble Polymers Regis™ 225104 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature 23.0 °C |
2.49 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® 7304 NC010 Nylon 6
(Unverified Data**) Zytel® 7304 NC010 is a medium viscosity, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.20 mm, Temperature -18.0 °C |
2.49 ft-lb/in @Thickness 0.126 in, Temperature -0.400 °F |
ASTM-D256 |
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -20.0 °C |
2.50 ft-lb/in @Temperature -4.00 °F |
1/8'' notched bar; ASTM D256 |
Ineos N07N-00 Polypropylene Impact Copolymer This is a medium melt flow rate, nucleated and antistatic impact copolymer polypropylene for injection molding applications that require a superior stiffness to impact balance.ApplicationsMaterials .. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature 23.0 °C |
2.49 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp PFL34 PA 6 LNP* Lubricomp* PFL34 is a compound based on Nylon 6 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am.. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.50 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF30 IM HS L 30% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI.. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.50 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 IM5 BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature 22.8 °C |
2.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced Notes: Impact Modified; Reinforced with 13% Glass Fibers; Synergistic compound exhibiting impact strength and dimensional stability Features: Good Dimensional stability; Good Processability; Heat St.. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.50 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/66 IM3 BK Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Copolymer, Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection Moldi.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.49 ft-lb/in @Temperature -40.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl 731H PPE+PS High gloss, general purpose grade. 130C (266F) DTUL. UL 94 HB rated. For multiple plugs, wine filter plates, etc.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature 0.000 °C |
2.50 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
Formosa Plastics Formolene® 6600A Impact Copolymer Polypropylene Impact Copolymer for Extrusion and Compounding Applications (Fractional Melt Flow) Formolene® 6600A is a high impact copolymer with an excellent balance of toughness and stiffness. It is suitable f.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature 25.0 °C |
2.50 ft-lb/in @Temperature 77.0 °F |
ASTM D256A |
Formosa Plastics Formolene® 6535N Impact Copolymer Polypropylene Impact Copolymer - Designed to Meet the Physical Requirements of Automotive Interior Trim Formolene® 6535N is an engineered, medium impact copolymer polypropylene. It was specifically developed to.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature 0.000 °C |
2.50 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
Formosa Plastics Formolene® 6613N Impact Copolymer Polypropylene Copolymer for Injection Molded Applications Requiring a Combination of High Toughness and Stiffness Formolene® 6613N is a copolymer of polypropylene designed and formulated for injection molding ap.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Clariant PA233 Nylon 6, Improved Processability, Easily Colorable, Toughened Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Clariant Renol PA233HT Nylon 6, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.50 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall 9211 Rigid PVC, Molding Georgia Gulf 9211 is a food grade vinyl compound designed to maximize clarity. It is suitable for use in a variety of food, cosmetic and personal care products.Information provided by Georgia GulfG.. |
|||
Izod Impact, Notched | >= 1.33 J/cm @Temperature -20.0 °C |
>= 2.50 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Buckeye Polymers BP FLEX D7030 BLK Thermoplastic Elastomer TPV Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.50 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall 8132 Rigid PVC, Extrusion Georgia Gulf 8132 is a rigid PVC compound designed for applications where transparency is important. This product remains unchanged except for the coded name and was previously identified as 3132. .. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature 23.0 °C |
2.49 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 3.17 mm |
2.50 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 5006 Rigid PVC, Extrusion, Natural Georgia Gulf 5006 Natural is a rigid PVC pellet compound designed for extrusion of interior rigid PVC profiles and various contours where high gloss and ease of processing is required. Georgia Gulf.. |
|||
Izod Impact, Notched | 1.33 J/cm @Thickness 6.35 mm |
2.50 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 9017J Clear 06 Rigid PVC, Molding, Clear Georgia Gulf 9017J Clear 06 is for food packaging and personal care applications requiring optimum taste and odor properties. The compound contains an ultraviolet light stabilizer, which protects l.. |
|||
Izod Impact, Notched | 1.33 J/cm @Temperature -40.0 °C |
2.49 ft-lb/in @Temperature -40.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl EN212 PPE+PS Extrusion grade. 212F (100C) DTUL. UL94 V-1 rated.This data was supplied by SABIC-IP for the Americas region. |