Material Notes:
Georgia Gulf 9209 is a food grade compound containing excellent optical and processing characteristics. It is suitable for use in a variety of food, cosmetic and general purpose packaging applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.4 MPa
6300 psi
ASTM D-638
Tensile Modulus 2.69 GPa
390 ksi
ASTM D-638
Flexural Strength 79.3 MPa
11500 psi
ASTM D-790
Izod Impact, Notched 1.39 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
2.60 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D-256
9.61 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
18.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Tensile Impact Strength 185 kJ/m²
88.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 62.00 °C
143.6 °F
ASTM D-648
Optical Properties Metric English Comments
Haze 5.0 %

@Thickness 3.17 mm
5.0 %

@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
Transmission, Visible 80 %

@Thickness 3.17 mm
80 %

@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
Descriptive Properties Value Comments
Equilibrium Torque, meter-grams 1400
Brabender Plastograph, No. 6 Roller Head, 190°C Bath, 57-g. Charge; 60/43 rpm
Stability Time, minutes 36