Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 143.6 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 62.00 °C
143.6 °F
annealed; ASTM D-648
Axiall 9246 Rigid PVC, Molding
Georgia Gulf 9246 is a high impact compound suitable for food packaging.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Deflection Temperature at 1.8 MPa (264 psi) 62.00 °C
143.6 °F
ASTM D-648
Axiall 9209 Rigid PVC, Molding
Georgia Gulf 9209 is a food grade compound containing excellent optical and processing characteristics. It is suitable for use in a variety of food, cosmetic and general purpose packaging applicati..
Deflection Temperature at 1.8 MPa (264 psi) 62.00 °C
143.6 °F
ASTM D-648
Axiall 9113 White 02 Rigid PVC, Molding, White 02
Georgia Gulf 9113 White 02 is a pre-colored white material with outstanding impact strength and processing properties. It is especially suited for packaging charcoal lighter fluid.Information provi..