Material Notes:
Georgia Gulf HF-6597 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of electrical and appliance applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D-785
Tensile Strength at Break 36.42 MPa
5282 psi
ASTM D-638
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Elongation at Break 139.2 %
139.2 %
ASTM D-638
Tensile Modulus 2.69 GPa
390 ksi
ASTM D-638
Flexural Strength 67.6 MPa
9800 psi
ASTM D-790
Flexural Modulus 2.48 GPa
360 ksi
ASTM D-790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm,
Temperature -20.0 °C
1.50 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D-256
8.01 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Gardner Impact 14.7 J

@Temperature 23.0 °C
10.8 ft-lb

@Temperature 73.4 °F
1/2" R Tup, 65 mil
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.00 °C
161.6 °F
ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D-648
UL RTI, Electrical 90.0 °C

@Thickness 1.50 mm
194 °F

@Thickness 0.0591 in
UL-746B
UL RTI, Mechanical with Impact 85.0 °C

@Thickness 1.50 mm
185 °F

@Thickness 0.0591 in
UL-746B
UL RTI, Mechanical without Impact 90.0 °C

@Thickness 1.50 mm
194 °F

@Thickness 0.0591 in
UL-746B
Flammability, UL94 5VA
5VA
Oxygen Index 36 %
36 %
ASTM D-2863
Descriptive Properties Value Comments
Flow Ratio (Distance/Wall Thickness, 390-400°F) 230
Georgia Gulf Test
UL Weatherability Rating F(1)
UL-746C