Axiall HH-2000 Rigid PVC, Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall HH-2000 Rigid PVC, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf HH-2000 is a high heat/high flow injection molding grade PVC alloy with a price/performance niche between high flow vinyl and utility engineering thermoplastics. It combines excellent flow, toughness and heat deflection/sag characteristics that are a marked improvement over standard vinyl. In addition, HH-2000 has excellent heat and light stability, color hold and surface appearance, making it an ideal candidate for Class A appearance parts requiring good heat warpage resistance such as color computer monitor housings. Process Note: Drying of material for 24 hours at 140-160°F in a dehumidifying dryer is recommended to endure optimum processing characteristics.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D-785
Tensile Strength, Yield 43.4 MPa
6300 psi
ASTM D-638
Tensile Modulus 2.62 GPa
380 ksi
ASTM D-638
Flexural Strength 75.8 MPa
11000 psi
ASTM D-790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D-790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm,
Temperature -20.0 °C
1.00 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D-256
2.14 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
4.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Gardner Impact 0.294 J

@Temperature 23.0 °C
0.217 ft-lb

@Temperature 73.4 °F
per mil, 1/2" R Tup
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 76.00 °C
168.8 °F
ASTM D-648
Flammability, UL94 5VA
5VA
Oxygen Index 30 %
30 %
ASTM D-2863
Descriptive Properties Value Comments
Flow Ratio (Distance/Wall Thickness, 390-400°F) 210
Georgia Gulf Test