Axiall SP-6340 Rigid PVC, Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall SP-6340 Rigid PVC, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf SP-6340 is a rigid vinyl injection molding compound designed for fittings and parts of similar confiation where maximum burst strength is required. Georgia Gulf 6340 is ideally suited for large diameter fittings. Georgia Gulf 6340 is listed with NSF under Standard 14, and meets Standard 61 health effects requirements.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D-785
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D-638
Tensile Modulus 2.90 GPa
420 ksi
ASTM D-638
Flexural Strength 75.8 MPa
11000 psi
ASTM D-790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D-790
Izod Impact, Notched 0.374 J/cm

@Thickness 3.17 mm,
Temperature -20.0 °C
0.700 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D-256
0.747 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.40 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Gardner Impact 36.2 J

@Temperature 23.0 °C
26.7 ft-lb

@Temperature 73.4 °F
1/2" R Tup125 mil
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 74.00 °C
165.2 °F
ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D-648
Oxygen Index 38 %
38 %
ASTM D-2863
Descriptive Properties Value Comments
Cell Classification, ASTM D-1784 12454-B
NSF std. 14
Flow Ratio (Distance/Wall Thickness, 390-400°F) 150
Georgia Gulf Test