Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall Suprel® SVA 9812 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name Suprel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall Suprel® SVA 9812 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf Suprel® SVA 9812 Alloy is an extrusion grade thermoplastic designed for sheet or profile applications requiring high impact resistance. Key features of Suprel 9812 alloy are flame retardance and excellent toughness at both room temperature and low temperatures. Suprel 9812 has good extrusion characteristics including good thermal stability and high gloss. It is particularly well suited for profile extrusion because the combination of low die swell, good melt strength and good melt stiffness allow easy sizing of extruded profiles. Suprel 9812 alloy is available in a full range of colors, or as un-pigmented "natural" for coloring on-line with concentrates. Typical applications include extruded sheet or profiles for use in construction, automotive, recreation, telecommunications or electrical products. Suprel 9812 can be used in exterior, weatherable applications if appropriate pigmentation is included.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
15 Seconds Delay; ASTM D-2246
79
79
Instantaneous; ASTM D-2246
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D-638
Tensile Modulus 2.32 GPa
337 ksi
ASTM D-638
Flexural Strength 63.4 MPa
9200 psi
ASTM D-790
Flexural Modulus 2.25 GPa
327 ksi
ASTM D-790
Izod Impact, Notched 4.27 - 5.87 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
8.00 - 11.0 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D-256
8.54 J/cm

@Thickness 3.17 mm,
Temperature 22.2 °C
16.0 ft-lb/in

@Thickness 0.125 in,
Temperature 72.0 °F
ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.2 °C
180 °F
annealed; ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C
180 °F
annealed; ASTM D-648
Vicat Softening Point 97.8 °C
208 °F
annealed; ASTM D-1525A
UL RTI, Electrical 50.0 °C
122 °F
UL-746B
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Flame Spread Index 35
35
RP; ASTM E-162
Users viewing this material also viewed the following: