Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746 |
PolyOne Geon™ Vinyl Rigid Molding M3890 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics GELOY CR7020 ASA ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746 |
PolyOne Geon™ HTX M6230 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
UL RTI, Electrical | 50.0 - 130 °C | 122 - 266 °F | Average value: 95.0 °C Grade Count:14 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics GELOY CR7520 ASA General purpose ASA. Excellent weatherability, good flow/aesthetics and high impact. Rated F2 by UL. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Geloy CR7520 ASA (Europe-Africa-Middle East) Geloy CR7520 is a general purpose injection moulding grade, blend of ASA/SAN. It can be positioned for outside parts in various markets, such as telecommunication, transportation, B&C, lighting and .. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL746B |
Idemitsu Kosan Xarec® N WA 5030 SPS, 30% Glass Filled |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=0.750 mm |
122 °F @Thickness >=0.0295 in |
|
LG Chemical LUCEL GC210 POM+GF10%, High Rigidity Feature: Injection Molding, POM+GF10%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness 1.57 - 6.33 mm |
122 °F @Thickness 0.0618 - 0.249 in |
|
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness 1.60 mm |
122 °F @Thickness 0.0630 in |
UL746B |
Ineos ABS Lustran® SAN Sparkle Highest-Clarity |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Noryl PX5622 PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. Good flow and surface aesthetics. UL94 V0/5VA/5VB. RTI Elec/Imp/Str 65. Suitable for E/E market indoor/outdoor applications.This da.. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific) Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Asia Pacific) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Noryl V180HF PPE+HIPS (Europe-Africa-Middle East) NORYL V180HF is an unfilled, flame retardant material. It has been fully optimized w.r.t. flow and is halogen free according to VDE/DIN 472 part 815.This data was supplied by SABIC-IP for the Europe.. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC1010 PPE+PS LNP* Stat-kon* Noryl_HMC1010 compound is a 10% Carbon fiber reinforced. Static dissipative. Nonbrominated, nonchlor- nated flame retardant system. UL94 V-1 rated. |
|||
UL RTI, Electrical | 50.0 °C @Thickness 1.50 mm |
122 °F @Thickness 0.0591 in |
UL 746 |
Teknor Apex APEX® 6500-80 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | |
Teknor Apex Elexar® EL 8732R Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL GFN1V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1V is a 10 % glass fibre reinforced material with a HDT/A of 110C according ISO 75. NORYL GFN1V cust spec 1977 has been approved for potable water applications up to 85C by the UK WFBS acco.. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PS+PA 30% Glass Reinforced PPE+PA Alloy. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP (Asia Pacific) PPE+PP blend. Suitable for painted exterior automotive applications. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL CTI2550 PPE+HIPS (Europe-Africa-Middle East) NORYL CTI2550 is a glass/mineral filled material with a Vicat B/120 of 160 °C according ISO 306. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Noryl PX1701 PPE+PS This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL-746B |
Axiall Suprel® SVA 9301 Rigid PVC, Molding Georgia Gulf Suprel® SVA 9301 is a general purpose injection molding alloy with mid-range properties, providing a balance of impact strength and stiffness and featuring excellent UL flammability li.. |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746 |
PolyOne Geon™ Vinyl Rigid Molding M4820 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL FN150 PPE+HIPS (Europe-Africa-Middle East) NORYL FN150 twin wall foam meets UL standard 94 V-0/5V ratings at 4 mm wall thickness. These unique flammability characteristics make FN150 the supreme choice for designing optimum wall thickness in.. |