Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 8.54 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 8.54 J/cm

@Temperature 22.8 °C
16.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC/TP-GP2 PC/Polyester Alloy
High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b..
Izod Impact, Notched 8.54 J/cm

@Temperature 22.8 °C
16.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC/TP-GP2-[color]-UV PC/Polyester Alloy, UV-stabilized
High Impact, Excellent Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
Izod Impact, Notched 8.54 J/cm

@Temperature 22.8 °C
16.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC/TP-GP3-IM PC/Polyester Alloy, Impact Modified
Superior Chemical Resistance, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide..
Izod Impact, Notched 8.54 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
16.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Lucent Polymers PC/PBT-1830 Polycarbonate+PBT, Superior Cold Temp Impact, Injection Grade
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Izod Impact, Notched 8.54 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
16.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Elastoblend® PA6/6 HI BK Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUl File Number: E157318Appearance: BlackProce..
Izod Impact, Notched 8.54 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
16.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Elastoblend® PA6/6 IM L W Nylon 66
Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc...
Izod Impact, Notched 8.54 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
16.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Elastoblend® PC E IM
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact Modified and High ViscosityProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Izod Impact, Notched 8.54 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
16.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Elastoblend® PC IM X
Availability: North AmericaForms: PelletsAdditive: Impact Modifier and Mold ReleaseFeatures: Impact Modified and Good Mold ReleaseProcessing Method: Injection MoldingInformation provided by TP Compo..
Izod Impact, Notched 8.54 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
16.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Plastiblend® PC/PBT IM 5727 BK
Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Notched 8.54 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
16.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Plastiblend® PC/PET IM 1016 UV
Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedInformation provided by TP Composites, Inc.
Izod Impact, Notched 8.54 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
16.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Elastoblend® PA6/6 IM L UV Nylon 66
Availability: North AmericaForms: PelletsAdditive: UV Stabilizer, Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP C..
Izod Impact, Notched 8.54 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
16.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Elastoblend® PA6/6 IM X Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP..
Izod Impact, Notched 8.54 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
16.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Elastoblend® PC IM
Availability: North AmericaForms: PelletsAdditive: Impact Modifier Features: Impact Modified Processing Method: Injection MoldingInformation provided by TP Composites, Inc.
Izod Impact, Notched 8.54 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
16.0 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Lubrizol ISOPLAST™ 2560 Engineering Thermoplastic Polyurethane Resin for Medical Applications
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaAvailableInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Izod Impact, Notched 8.54 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
16.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Lubrizol ISOPLAST™ 2560 Engineering Thermoplastic Polyurethane Resin for Medical Applications
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaAvailableInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Izod Impact, Notched 8.54 J/cm

@Temperature 22.8 °C
16.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Clariant PA233 Nylon 6, Improved Processability, Easily Colorable, Toughened
Data provided by Clariant Masterbatches
Izod Impact, Notched 8.54 J/cm

@Temperature 22.8 °C
16.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Clariant Renol PA233HT Nylon 6, Improved Processability, Easily Colorable, Highly Toughened
Data provided by Clariant Masterbatches
Izod Impact, Notched 8.54 J/cm

@Thickness 3.17 mm,
Temperature 22.2 °C
16.0 ft-lb/in

@Thickness 0.125 in,
Temperature 72.0 °F
ASTM D-256
Axiall Suprel® SVA 9812 Rigid PVC, Extrusion
Georgia Gulf Suprel® SVA 9812 Alloy is an extrusion grade thermoplastic designed for sheet or profile applications requiring high impact resistance. Key features of Suprel 9812 alloy are flame ret..
Izod Impact, Notched 8.54 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
16.0 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D-256
Axiall 7055 Rigid PVC, Extrusion