Material Notes:
Formula: C5H13NOCAS: 3179-63-3Description: 3-Dimethylaminopropane-1-ol is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: 1-Propanol, 3-(dimethylamino)- Dimethylpropanolamine, 3-(N,N-Dimethylamino)-1-propanol, 3-(Dimethylamino)propanol, 1-Dimethylamino-3-propanol, N,N-Dimethyl-3-aminopropanol, N,N-Dimethyl-3-hydroxypropylamine, N,N-DimethylpropanolamineApplications: Intermediate used in the production of Dyes, Pharmaceuticals and Ion exchangerInformation provided by BASF
Physical Properties Metric English Comments
Density 0.886 g/cc
0.0320 lb/in³
Molecular Weight 103.2 g/mol
103.2 g/mol
Thermal Properties Metric English Comments
Melting Point -35.0 °C
-31.0 °F
Boiling Point 159 °C
318 °F
Flash Point 54.0 °C
129 °F
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
DIN 51 777
Descriptive Properties Value Comments
Assay >99%
Color <50
APHA, DIN EN 1557
Ignition Temperature 235°C