Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Elastollan® 1154D Polyether Type Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer BASF
Trade Name Elastollan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan® 1154D Polyether Type Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exhibit excellent low temperature properties, hydrolysis resistance and fungus resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing.Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ASTM D2240
Tensile Strength, Ultimate 40.0 MPa
5800 psi
ASTM D412
Tensile Strength, Yield 20.0 MPa

@Strain 100 %
2900 psi

@Strain 100 %
ASTM D-412
30.0 MPa

@Strain 300 %
4350 psi

@Strain 300 %
ASTM D-412
Elongation at Break 460 %
460 %
ASTM D412
Tear Strength 180 kN/m
1030 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 75
75
H-18 wheel; ASTM D-1044.
Tensile Set 70 %
70 %
at break; ASTM D-412
Electrical Properties Metric English Comments
Comparative Tracking Index >= 600 V
>= 600 V
DIN/IRC 112