Mechanical Properties Metric English Comments
Tear Strength 180 kN/m
1030 pli
ISO 34B
Huntsman AVALON® 60 DB Thermoplastic Polyurethane
Introduction: AVALON 60 DB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DB is part of the AVALON Perform Range and offers a premium soling materi..
Tear Strength 180 kN/m
1030 pli
ASTM D1004
SK Chemicals SKYPEL G163D General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tear Strength 180 kN/m
1030 pli
ASTM D624
Wanhua Chemical Wanthane® WHT-1295B Polyester Based TPU
Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd.
Tear Strength 180 kN/m
1030 pli
without incision; ISO 34B
Lubrizol ESTANE® GP98AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 98AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Tear Strength 180 kN/m
1030 pli
parallel; ISO 34-1
DuPont Performance Polymers Hytrel® 7246HS BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers
Tear Strength 180 kN/m
1030 pli
parallel; ISO 34-1
DuPont Performance Polymers Hytrel® HTR8730 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Viscosity Polyester Elastomer with Excellent Mechanical Properties at Elevated Temperatures Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tear Strength 180 kN/m
1030 pli
DIN ISO 34-1/Bb
BASF Elastollan B 64 D TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup..
Tear Strength 180 kN/m
1030 pli
ASTM D624
BASF Elastollan® S98A Polyester Type Polyurethane Elastomer
Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv..
Tear Strength >= 180 kN/m
>= 1030 pli
ISO 34
Austin Novel Materials Texalan® 372D Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tear Strength 180 kN/m
1030 pli
DIN ISO 34-1/Bb
BASF Elastollan 560 D TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and a high abrasion resistance.Typical Applications: Heel top-pieces, castor tyres and parts requiri..
Tear Strength 180 kN/m
1030 pli
ASTM D624
BASF Elastollan® 1154D Polyether Type Polyurethane Elastomer
Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exh..
Copyright © lookpolymers.com All Rights Reserved