BASF Elastollan S 74 D TPUR

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer BASF
Trade Name Elastollan
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan S 74 D TPUR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applications: Shoe-soles, top pieces, tubes, technical parts e.g. castor tyres.Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°CInformation provided by BASF
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183-1-A
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
ISO 686
Tensile Strength 40.0 MPa
5800 psi
ISO 37
25.0 MPa

@Strain 20.0 %
3630 psi

@Strain 20.0 %
ISO 37
30.0 MPa

@Strain 100 %
4350 psi

@Strain 100 %
ISO 37
40.0 MPa

@Strain 300 %
5800 psi

@Strain 300 %
ISO 37
Elongation at Break 300 %
300 %
ISO 37
Charpy Impact, Notched 0.300 J/cm²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
DIN EN ISO 179
17.0 J/cm²

@Temperature 23.0 °C
80.9 ft-lb/in²

@Temperature 73.4 °F
DIN EN ISO 179
Tear Strength 240 kN/m
1370 pli
DIN ISO 34-1/Bb
Abrasion 25
25
[mm<sup>3</sup>; ISO 4649
Compression Set 55 %

@Temperature 23.0 °C
55 %

@Temperature 73.4 °F
ISO 815
60 %

@Temperature 70.0 °C
60 %

@Temperature 158 °F
ISO 815
Processing Properties Metric English Comments
Processing Temperature 175 - 240 °C
347 - 464 °F
Injection molding
Mold Temperature 20.0 - 70.0 °C
68.0 - 158 °F
Descriptive Properties Value Comments
Commercial Status North America
Primary Processing Technique Injection molding