BASF Heligoen® Blue K 6911 D Color Additive

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer BASF
Trade Name Heligoen®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Heligoen® Blue K 6911 D Color Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Structure: Cu-phthalocyanine alpha stabApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, PA, PETP, CA/CAB, and UPRecommendations for food applications: BgVV, FDA, FrancePhysical form: PowderInformation provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.330 g/cc
0.0119 lb/in³
Density 1.60 g/cc
0.0578 lb/in³
Specific Surface Area 81 m²/g
81 m²/g
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Electrical Properties Metric English Comments
Electrical Resistivity 5000 ohm-cm
5000 ohm-cm
Chemical Properties Metric English Comments
Total Acid Number 5.0 - 8.0
5.0 - 8.0
Descriptive Properties Value Comments
Chemical Fastness (months) H2SO4 10%
>6 months
H2SO4 conc.
>6 months
HCI 10%
>6 months
HCI conc.
Instable
HNO3 10%
>6 months
HNO3 conc.
Instable
Na2CO3 sat.
>6 months
NaOH conc.
>6 months
Color Blue
Light Fastness 8
Migration Fastness 5