Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Petra® 7010 WT 7729 15% Glass Filled PET

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 20% Glass Reinforced
Manufacturer BASF
Trade Name Petra®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Petra® 7010 WT 7729 15% Glass Filled PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Petra 7010 WT7729 is a 15% glass fiber reinforced, pigmented white injection molding compound based on post-consumer recycle polyethylene terephthalate. Formulated for superior surface aesthetics, it exhibits excellent melt stability and high flow over a broad range of processing conditions. The combination of high strength and dimensional stability enable its use in structural applications designed for metal.Application: Petra 7010 WT7729 is recommended for applications such as appliance door handles and knobs.Information provided by BASF
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
ISO 527
Elongation at Break 1.5 %
1.5 %
ISO 527
Flexural Modulus 6.80 GPa
986 ksi
ISO 178
Charpy Impact Unnotched 1.50 J/cm²

@Temperature 5.00 °C
7.14 ft-lb/in²

@Temperature 41.0 °F
ISO 179
Thermal Properties Metric English Comments
Melting Point 245 °C
473 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75
Processing Properties Metric English Comments
Melt Temperature 280 - 300 °C
536 - 572 °F
Mold Temperature 100 - 110 °C
212 - 230 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content 0.20 %
0.20 %
Descriptive Properties Value Comments
Color WT 7792
Commercial Status North America
Users viewing this material also viewed the following: