Category | Polymer |
Manufacturer | BASF |
Trade Name | PolyTHF® |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | BASF PolyTHF® 1000 Polyether.pdf |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.982 g/cc @Temperature 30.0 °C |
0.0355 lb/in³ @Temperature 86.0 °F |
|
Molecular Weight | 950 - 1050 g/mol | 950 - 1050 g/mol | 8892 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 26.0 °C | 78.8 °F | |
Boiling Point | >= 250 °C | >= 482 °F | |
Flash Point | >= 240 °C | >= 464 °F |
Chemical Properties | Metric | English | Comments |
---|---|---|---|
Total Acid Number | 0.050 | 0.050 | [mg KOH/g]; 8438 |
Descriptive Properties | Value | Comments |
---|---|---|
Color | <40 | APHA, 10605 |
Hydroxyl Number | 106.9-118.1 mg KOH/g | 8892 |
Stabilizer | 200-350 ppm | 8431 |