Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.982 g/cc | 0.0355 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 9007 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 0.983 g/cc | 0.0355 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA300 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive high strength.Information provided by Illinois Tool Works. |
|||
Density | 0.982 g/cc @Temperature 30.0 °C |
0.0355 lb/in³ @Temperature 86.0 °F |
|
BASF PolyTHF® 1000 Polyether Description: PolyTHF 1000 is a colorless, odorless waxy substance. It is soluble organic solvents.Applications: Intermediate used in the production of: Synthesis of elastomers, Spandex Fibers, TPU, .. |
|||
Density | 0.983 g/cc | 0.0355 lb/in³ | AboCure 50-12 |
Abatron AboCast 22-30/AboCure 50-12 Epoxy AboCast 22-30 is a black filled resin with high viscosity and a weight of 12.4 lbs/gallon. AboCure 50-12 is clear, fast converter with low viscosity and a weight of 8.2 lbs/gallon. AboCast 22-30/Abo.. |