BASF Procom® D 1153 Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer BASF
Trade Name Procom®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Procom® D 1153 Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 80.0 MPa
11600 psi
Elongation at Break 3.0 %
3.0 %
Tensile Modulus 7.50 GPa
1090 ksi
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
3.00 J/cm²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 60.0 µm/m-°C

@Temperature 20.0 °C
33.3 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
Deflection Temperature at 1.8 MPa (264 psi) 148 °C
298 °F
Vicat Softening Point 144 °C
291 °F
Users viewing this material also viewed the following: