BASF Ultramid® NFX-0102 NF2004 30% Glass Filled PA66 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® NFX-0102 NF2004 30% Glass Filled PA66 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ultramid NFX-0102 NF2004 is a heat stabilized, 30% glass bead PA66 injection molding grade. It is especially formulated for low warp, increased stiffness and excellent dimensional stability.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 70.0 MPa
10200 psi
5mm/min; ISO 527
Elongation at Break 2.5 %
2.5 %
5mm/min; ISO 527
Tensile Modulus 4.50 GPa
653 ksi
1mm/min; ISO 527
Flexural Modulus 4.20 GPa
609 ksi
ISO Data
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO Test
Charpy Impact, Notched 0.250 J/cm²
1.19 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 263 °C
505 °F
10 K/min
263 °C
505 °F
ASTM Test
Descriptive Properties Value Comments
Color Natural
Commercial Status Active America
Impact Modified No
Primary Processing Technique Injection Molding