Slo-Kast is a low viscosity, medium setting, easy to use casting material. This polyurethane system features extremely low shrinkage when properly cured. Unlike Kwik-Kast, BC 8009 offers the user longer working time for filling large closed mold cavities. Slo-Kast is ideal for casting large sections without having to stage pour. Uses include; tracing models, core boxes, keller aids, patterns, core sticks, vacuum form tools, prototypes and display parts.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.80 - 1.90 g/cc
1.80 - 1.90 g/cc
ASTM D792-66
Brookfield Viscosity 2950 cP

@Temperature 23.9 °C
2950 cP

@Temperature 75.0 °F
#3 spindle @ 20 rpm; ASTM D2393
Linear Mold Shrinkage 0.00020 cm/cm
0.00020 in/in
ASTM D2566-69
Mechanical Properties Metric English Comments
Hardness, Shore D 85

@Temperature 23.9 °C
85

@Temperature 75.0 °F
ASTM D2240
Tensile Strength, Ultimate 40.3 MPa
5850 psi
Compressive Strength 60.7 MPa
8800 psi
ASTM D695
Processing Properties Metric English Comments
Cure Time 210 - 240 min

@Temperature 24.0 °C
3.50 - 4.00 hour

@Temperature 75.2 °F
demold time
Pot Life 14 - 17 min

@Temperature 24.0 °C
14 - 17 min

@Temperature 75.2 °F
1 lb. mass
Descriptive Properties Value Comments
Mix Ratio 1:1 by weight or volume