Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 14 - 15 min @Temperature 24.0 °C |
14 - 15 min @Temperature 75.2 °F |
1/2 lb mass |
BCC Products BC 5003 Epoxy Laminating System BC 5003 is a medium viscosity, unfilled laminating system. It is a room temperature curing resin with a relatively short pot life. BC 5003 is also considered an excellent general purpose adhesive fo.. |
|||
Pot Life | 14 - 17 min @Temperature 24.0 °C |
14 - 17 min @Temperature 75.2 °F |
1 lb. mass |
BCC Products SLO-KAST BC 8009 Urethane Casting Slo-Kast is a low viscosity, medium setting, easy to use casting material. This polyurethane system features extremely low shrinkage when properly cured. Unlike Kwik-Kast, BC 8009 offers the user lo.. |