BLUESTAR 101G20 PBT, 20% Glass Filled

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Manufacturer BLUESTAR
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BLUESTAR 101G20 PBT, 20% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Applications: Appliances, molded partsInformation provided by Polymer Technology and Services, LLC (PTS).
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.12 %
0.12 %
50% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
ASTM D955
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 250 °C
18 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 95.0 MPa
13800 psi
ASTM D638
Tensile Modulus 7.10 GPa
1030 ksi
ASTM D638
Flexural Strength 165 MPa
23900 psi
ASTM D790
Flexural Modulus 6.85 GPa
994 ksi
ASTM D790
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
ASTM D256
Izod Impact, Unnotched (ISO) 43.0 kJ/m²
20.5 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
ASTM D648
Flammability, UL94 HB

@Thickness 0.380 mm
HB

@Thickness 0.0150 in
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in