Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BLUESTAR LXS 312 PPE-HIPS, 20% Mineral Filled

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS) , Polystyrene + Polyphenylene Ether, Glass + Mineral Filler
Manufacturer BLUESTAR
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BLUESTAR LXS 312 PPE-HIPS, 20% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Applications: LED shellInformation provided by Polymer Technology and Services, LLC (PTS).
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Water Absorption 0.10 %

@Temperature 23.0 °C,
Time 86400 sec
0.10 %

@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 30 g/10 min

@Load 5.00 kg,
Temperature 300 °C
30 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
type I; ASTM D638
Elongation at Break 40 %
40 %
type I; ASTM D638
Flexural Strength 82.0 MPa
11900 psi
2.6 mm/min; ASTM D790
Flexural Modulus 2.30 GPa
334 ksi
2.6 mm/min; ASTM D790
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 120 °C

@Thickness 6.40 mm
248 °F

@Thickness 0.252 in
ASTM D648
Users viewing this material also viewed the following: