Material Notes:
Description: Multipurpose extrusion/injection resin with excellent processability and good stiffness. This resin meets the Food and Drug Administration requirements for food contact applications.Applications: Profiles, Tubing, Small Bottles, Caps and Closures.Information provided by Bamberger Polymers.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D-1505
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 47
47
ASTM D-2240
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM D-638
Elongation at Break 600 %
600 %
ASTM D-638
Modulus of Elasticity 0.186 GPa
27.0 ksi
ASTM D-638
Flexural Modulus 0.179 GPa
26.0 ksi
ASTM D-790
Izod Impact, Notched NB
NB
ASTM D-256
Descriptive Properties Value Comments
Process Extrusion
Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved