Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Barlog Plastics KEBAFORM C 902 CF POM Copolymer, carbon fiber reinforced, electr. conductive

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Carbon Fiber Filled
Manufacturer Barlog Plastics
Trade Name KEBAFORM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBAFORM C 902 CF POM Copolymer, carbon fiber reinforced, electr. conductive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
POM-CF10Information provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ISO 1183
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
ISO 527-1
Elongation at Break 4.0 %
4.0 %
ISO 527-1
Tensile Modulus 6.60 GPa
957 ksi
ISO 527-1
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179-1eA
Thermal Properties Metric English Comments
Melting Point 166 °C
331 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1e+05
1e+05
IEC 60093
Surface Resistance 10000 ohm
10000 ohm
IEC 60093
Descriptive Properties Value Comments
Resin Type POM-CF10