Polymer Property : Charpy Impact, Notched = 2.14 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer
Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr..
Charpy Impact, Notched 0.450 J/cm² - NB

@Temperature -40.0 - -30.0 °C
2.14 ft-lb/in² - NB

@Temperature -40.0 - -22.0 °F
Average value: 5.40 J/cm² Grade Count:46
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..
Charpy Impact, Notched 0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DuPont Performance Polymers Crastin® S600F20 BK851 PBT  (Unverified Data**)
Crastin® S600F20 BK851 is an unreinforced, lubricated, medium viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DuPont Performance Polymers Crastin® S600F40 BK851 PBT  (Unverified Data**)
Crastin® S600F40 BK851 is an unreinforced, lubricated, low viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Victrex® PEEK 90G Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c..
Charpy Impact, Notched 0.450 J/cm² - NB
2.14 ft-lb/in² - NB
Average value: 4.74 J/cm² Grade Count:102
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
IRPC Polimaxx Polene 2346S Polypropylene Block Copolymer
CHARACTERISTICS: HIGH STIFFNESS, HIGH FLOW, GOOD IMPACT, HEAT STABILITY CONTAIN ANTISTATIC AND UV STABILIZER ADDITIVEAPPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES, AUTOPARTS
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
LATI Larton K/30 PPS, 30% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
LATI Latamid 66 H2 G/25-V0CT4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Lat..
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179/1EA-1993
Solvay Technyl® A 205F Nylon 66, EH0
Unreinforced polyamide 66, high fluidity, fast cycling grade, for injection molding.Technyl A 205F offers two main advantages: excellent filling qualities and UL 94 V2 under 0.4 mm. It is particula..
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179/1eA
Polyplastics FR-PET® C3015FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
Information provided by PolyPlastics.
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179
Total PPH 7062 Polypropylene, Homopolymer
ATOFINA Polypropylene PPH 7062 is an antistatic homopolymer.ApplicationATOFINA Polypropylene PPH 7062 is intended for injection molding applications of boxes, closures and household articles. Inform..
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179
Total PPH 7069 Polypropylene, Homopolymer
ATOFINA Polypropylene PPH 7069 is homopolymer.ApplicationATOFINA Polypropylene PPH 7069 is characterized by medium fluidity for extrusion of continuous filament (CF) and bulk continuous filament (BC..
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179
Total PPH 7089 Polypropylene Homopolymer, Fiber
Polypropylene PPH 7089 is a narrow molecular weight distribution homopolymer polypropylene, with anti-gas fading stabilization.Polypropylene PPH 7089 is intended for the extrusion of fibers with the..
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis Bormod™ BF970MO Polypropylene for Injection Molding
Bormod BF970MO is a heterophasic copolymer characterized by an optimum combination of very high stiffness and high impact strength.Bormod BF970MO is a new generation grade for very fast production o..
Charpy Impact, Notched 0.450 - 0.550 J/cm²
2.14 - 2.62 ft-lb/in²
ISO 179
Vyncolit 2950 W Novolac Phenolic
Mineral and glass fiber filled phenolic molding compound with a very high strain to failure in flexure. UL listed.USES: Armature insulation.Information provided by Vyncolit, a Sumitomo Bak Group
Charpy Impact, Notched 0.450 J/cm²

@Temperature -40.0 °C
2.14 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® 330 NC010 Nylon  (Unverified Data**)
Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179-1eA
Barlog Plastics KEBAFORM C 902 CF POM Copolymer, carbon fiber reinforced, electr. conductive
POM-CF10Information provided by BARLOG plastics GmbH.
Charpy Impact, Notched 0.450 J/cm²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYfill PPHC K8020 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Charpy Impact, Notched 0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYfill PPHC K8030 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Charpy Impact, Notched 0.450 J/cm²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 2440 K Polypropylene
Data was collected by ISO methods and provided by BASF.
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179
BASF Nypel® 2367G HS BK 15/25% Glass/Mineral Filled PA6 (Dry)
Nypel 2367G HS BK-4 is a black pigmented, heat stabilized, 40% mineral and glass fiber reinforced injection molding compound based on recycled PA6 feedstocks. It possesses a balance of engineering ..
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179/1eA
Polyplastics Duracon® CH-15 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
IRPC Polimaxx Polene 2340S Polypropylene Block Copolymer
CHARACTERISTICS: HIGH FLOW, HIGH STIFFNESS, HEAT STABILITY, GOOD IMPACTAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES, THIN WALL PARTS
Charpy Impact, Notched 0.450 J/cm²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont ..