Beijing Evergrow Resources UHMW PE Bar

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Beijing Evergrow Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Evergrow Resources UHMW PE Bar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:Engineering manufacture:gear wheel, bearing bushes, sliding elements, chute liners, bunker liners, chain wear strip, guide strips and liners. The paper industry:suction box covers and guiding strips.The textile industry:lug straps, picker sticks, loom pickers, picker shields and spinning and mooring rope etc. The food handling equipment:cutting boards, kitchen work tops and wear parts.Machine construction: spray nozzles, agitator screws, acid pump impellers and valve liners.MiningInformation provided by Beijing Evergrow Resources.
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 24.0 MPa
>= 3480 psi
Elongation at Break 140 %
140 %