Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Blue River Coatings
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Blue River Coatings High Performance Acrylic Sanding Sealer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BLUE RIVER COATINGS HIGH PERFORMANCE ACRYLIC SANDING SEALER is a waterbased wood sealer to fill the grain. The product is designed to be a sandable self-sealing topcoat for wood. HIGH PERFORMANCE ACRYLIC SANDING SEALER offers good application properties, low foam, good adhesion, and excellent sanding properties. HIGH PERFORMANCE ACRYLIC SANDING SEALER dries quickly (eliminating excessive grain raise on wood) and provides excellent sealing properties to help repel water. The product is designed to work in conjunction with Blue River Coatings Wood Stains and Topcoats.Enviromental Advantages:BLUE RIVER COATINGS HIGH PERFORMANCE ACRYLIC SANDING SEALER is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated, dried and sent to a “Class B” landfill. Check with local and state regulations for proper handling. Characteristics:Excellent grain fillerMinimal grain raisingDry to touch in 15 minutes and Dry to sand in 30 minutes at 70°F and 50% humidityCan be applied in a wide variety of temperature and humidity conditionsWater is used for clean-upNon-HazardousShelf life of 1 yearNon-FlammableUsesAny wood surface that can be sanded, stained, or selaedInformation provided by Blue River Coatings
Physical Properties Metric English Comments
Specific Gravity >= 1.00 g/cc
>= 1.00 g/cc
Density 1.04 g/cc
0.0377 lb/in³
Solids Content 39.2 %
39.2 %
by volume
43 %
43 %
by weight
Volatile Organic Compounds (VOC) Content 144 g/l
144 g/l
Thermal Properties Metric English Comments
Boiling Point 169 °C
336 °F
Flash Point 65.6 °C
150 °F
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 75.0 °C
0.167 hour

@Temperature 167 °F
Recoat, at 50% humidity
19.8 min

@Temperature 75.0 °C
0.330 hour

@Temperature 167 °F
Dust Free, at 50% humidity
45.0 min

@Temperature 75.0 °C
0.750 hour

@Temperature 167 °F
Dry to handle, at 50% humidity and 75°C
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Flexibility Good
Pencil Hardness HB
Theoretical Coverage 642 ft2 at 1 mil