Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Lexan® FXE171R PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Lexan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Lexan® FXE171R PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LEXAN FXE171R is a transparent/translucent high flow grade for special effects colors with a fluorescent appearance. Color package may affect performance.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Moisture Absorption 0.150 %
0.150 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %
0.35 %
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
on Tensile Bar; SABIC Method
Melt Index of Compound 26 g/10 min

@Load 1.20 kg,
Temperature 300 °C
26 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Hardness, H358/30 95.0 MPa
13800 psi
ISO 2039-1
Tensile Strength at Break 50.0 MPa
7250 psi
50 mm/min; ISO 527
Tensile Strength, Yield 63.0 MPa
9140 psi
50 mm/min; ISO 527
Elongation at Break 70 %
70 %
50 mm/min; ISO 527
Elongation at Yield 6.0 %
6.0 %
50 mm/min; ISO 527
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
Flexural Yield Strength 90.0 MPa
13100 psi
2 mm/min; ISO 178
Flexural Modulus 2.30 GPa
334 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 60.0 kJ/m²
28.6 ft-lb/in²
80*10*3; ISO 180/1A
11.0 kJ/m²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*3; ISO 180/1U
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
80*10*3; ISO 180/1U
Charpy Impact Unnotched NB
NB
Edgew 80*10*3 sp=62mm; ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 6.00 J/cm²
28.6 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 133 °C
271 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 139 °C
282 °F
Rate B/50; ISO 306
140 °C
284 °F
Rate B/120; ISO 306
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
transparent/translucent; thickness not quantified
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASSES
IEC 60695-10-2