Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis BorECO™ BA2000 Polypropylene Block Copolymer for Non-Pressure Pipes

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name BorECO™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BorECO™ BA2000 Polypropylene Block Copolymer for Non-Pressure Pipes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BorECO™ BA2000 is a high molecular weight, low melt flow rate polypropylene block copolymer with a good balance of mechanical properties. This grade offers superior stiffness while keeping good impact resistance and shows excellent processability. Applications: BorECO™ BA2000 is recommended for solid wall gravity pipes in the application filed of: underground drainage, sewerage, soil, and waste.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 38.0 MPa
5510 psi
50mm/min; ISO 527-2
Elongation at Yield 6.5 %
6.5 %
50mm/min; ISO 527-2
Flexural Modulus 2.00 GPa
290 ksi
1mm/min; ISO 178
Charpy Impact, Notched 0.200 J/cm²

@Temperature -20.0 °C
0.952 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
2.90 J/cm²

@Temperature 23.0 °C
13.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Processing Properties Metric English Comments
Middle Barrel Temperature 200 - 220 °C
392 - 428 °F
cylinder
Die Temperature 210 - 220 °C
410 - 428 °F
Melt Temperature 210 - 230 °C
410 - 446 °F
Head Temperature 210 - 230 °C
410 - 446 °F