Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 200 °C | 392 °F | Zone 5; Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 7100 PRE-ELEC ESD 7100 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7100 has been developed for inject.. |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL EI5002L PP Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 9002-88-4Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP2100 PP+GF10% Description: Injection Molding, PP+GF10%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3202 PP+MF20% Description: Injection Molding, PP+MF10%, General Purpose, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG.. |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL HG3200SK2 PP+MF20%, High Gloss Description: Injection Molding, PP+MF20%, High GlossApplication: Electrical & Electronic PartsCAS: 9003-07-0 and 7727-43-7Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical MP220 ABS, High Adhesion, Heat Resistance Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | |
LG Chemical LUPOL GP-3152F General Purpose Polypropylene, 15% Mineral Fillers, High Impact, Flame Retardant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3400 PP+MF40% Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | |
LG Chemical LUPOL HF-3308 High Flow Polypropylene, 30% Mineral Fillers LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | |
LG Chemical LUPOL TE-5006K Thermoplastic Elastomer Alloy, Weather Resistant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Middle Barrel Temperature | 200 - 240 °C | 392 - 464 °F | |
Sumitomo Chemical ESPOLEX® 3255 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 200 - 240 °C | 392 - 464 °F | |
Sumitomo Chemical ESPOLEX® 3785 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 200 - 245 °C | 392 - 473 °F | |
Sumitomo Chemical ESPOLEX® WT521 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | cylinder |
Borealis BorECO™ BA2000 Polypropylene Block Copolymer for Non-Pressure Pipes BorECO™ BA2000 is a high molecular weight, low melt flow rate polypropylene block copolymer with a good balance of mechanical properties. This grade offers superior stiffness while keeping good im.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | cylinder |
Borealis BorECO™ BA415E Polypropylene Block Copolymer for Non-Pressure Pipes BorECO™ BA415E is a high molecular weight, low melt flow rate polypropylene block copolymer with high stiffness and impact strength. This material has been designed for improved processability and.. |
|||
Middle Barrel Temperature | 200 - 250 °C | 392 - 482 °F | |
Diamond Polymers ABS 4000HH Description: Heat Resistant Grade, Medium High HeatInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 200 - 250 °C | 392 - 482 °F | |
Diamond Polymers ABS TM 25 Description: Heat Resistant Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |