Borealis Bormed™ DM55pharm Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Borealis
Trade Name Bormed™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Bormed™ DM55pharm Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bormed™ DM55pharm is a low melt flow rate polypropylene homopolymer intended for extrusion and thermoforming. Its very good organoleptic properties allows this grade to be used with any master batch without discoloring problems. Applications: Bormed™ DM55pharm is recommended for in line and off line thermoforming, pharmaceutical and medical device packaging, pharmaceutical blisters, and food packaging.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 2.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
50mm/min; ISO 527-2
Elongation at Yield 9.0 %
9.0 %
50mm/min; ISO 527-2
Tensile Modulus 1.60 GPa
232 ksi
1mm/min; ISO 527-2
Flexural Modulus 1.50 GPa
218 ksi
5mm/min; ISO 178
Thermal Properties Metric English Comments
Melting Point 162 - 166 °C
324 - 331 °F
ISO 3146
Optical Properties Metric English Comments
Haze 27 %
27 %
ASTM D1003