Material Notes:
HC207TF is a special nucleated polypropylene homopolymer intended for thermoforming packaging. Applications: HC207TF is recommended for in-line and off line thermoforming, high transparent trays, cups and containers, housewares and thin wall packaging, margarine tubs and dairy containers, and blending with copolymers for lids. HC207TF contains antistatic agents for protection against dust and dirt pick up.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 2.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Modulus 1.70 GPa
247 ksi
1mm/min; ISO 527-2
Flexural Modulus 1.65 GPa
239 ksi
2mm/min; ISO 178
Charpy Impact, Notched 0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 163 - 167 °C
325 - 333 °F
DSC; ISO 3146
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 210 - 240 °C
410 - 464 °F