Material Notes:
MG9601 is a natural high-density polyethylene with high melt-index and narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. The grade is characterized by excellent flow properties, minor distortion and high stiffness. Applications: House ware and thin wall packaging.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 31 g/10 min

@Load 2.16 kg,
Temperature 190 °C
31 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ISO 868
Tensile Strength, Yield 25.0 MPa
3630 psi
50mm/min; ISO 527-2
Elongation at Yield 9.0 %
9.0 %
50mm/min; ISO 527-2
Tensile Modulus 1.05 GPa
152 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.300 J/cm²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
0.300 J/cm²

@Temperature -20.0 °C
1.43 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 71.0 °C
160 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 180 - 240 °C
356 - 464 °F
Mold Temperature 10.0 - 40.0 °C
50.0 - 104 °F
Descriptive Properties Value Comments
Hold Pressure as low as possible
Injection Velocity as high as possible