Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis Superclean™ LR4201S Crosslinkable Polyethylene Insulation for Medium and High Voltage Power Cables

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Wire/Cable Grade
Manufacturer Borealis
Trade Name Superclean™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Superclean™ LR4201S Crosslinkable Polyethylene Insulation for Medium and High Voltage Power Cables.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Superclean LR4201S is a Superclean crosslinkable low density polyethylene (XLPE) for medium and high voltage power cable insulation. The formulation of LR4201S provides an optimum combination of good extrudability and electrical properties. LR4201S is natural in color.LR4201S has been specifically developed for medium and high voltage power cables. Because it is a Superclean material, LR4201S is suitable for use in high voltage cables rated up to 161 kV.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
Base Resin; ASTM D1928/D 1505
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
ASTM D1693
ESCR 10% Igepal® >= 1000 hour
>= 1000 hour
ASTM D1693
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Base Resin; ISO 1133
Degree of Crosslinking 12 %
12 %
ASTM D2765
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
ASTM D2240
Tensile Strength, Yield >= 13.7 MPa
>= 1980 psi
Heat Aging (168 hrs at 136°C); ASTM D638
15.2 MPa
2200 psi
At 20 in/min; ASTM D1238
Elongation at Break <= 75 %
<= 75 %
Hot Creep Test (150°C,29 psi); ICEA T-28-562
400 %
400 %
ASTM D638
Tensile Set 5.0 %
5.0 %
Hot Creep Test (150°C,29 psi); ICEA-T-28-562
360 %
360 %
Retention; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 2.3

@Frequency 60 Hz
2.3

@Frequency 60 Hz
ASTM D150
Dielectric Strength >= 21.7 kV/mm

@Thickness 1.30 mm
>= 550 kV/in

@Thickness 0.0512 in
ASTM D149
Dissipation Factor 0.00050

@Frequency 60 Hz
0.00050

@Frequency 60 Hz
ASTM D150