Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem F2523 Blown Film Extrusion Low Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem F2523 Blown Film Extrusion Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Automatic packaging for several products; High transparency films.Additives: Antiblock, DInformation provided by Braskem.
Physical Properties Metric English Comments
Specific Gravity 0.923 g/cc
0.923 g/cc
ASTM D1505/D792
Thickness 25.0 microns
0.984 mil
Melt Flow 2.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 230 %
230 %
ASTM D882
Film Elongation at Break, TD 930 %
930 %
ASTM D882
Elmendorf Tear Strength TD 110 g
110 g
gF; ASTM D1922
Dart Drop Test 60.0 g
0.132 lb
gF/50%f; ASTM D1709
Film Tensile Strength at Break, MD 30.0 MPa
4350 psi
ASTM D882
Film Tensile Strength at Break, TD 20.0 MPa
2900 psi
ASTM D882
Optical Properties Metric English Comments
Haze 6.0 %

@Thickness 0.0250 mm
6.0 %

@Thickness 0.000984 in
ASTM D1003
Gloss 110 %

@Thickness 0.0250 mm
110 %

@Thickness 0.000984 in
60°; ASTM D2457