Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TS 7010 LDPE - Medium Duty Packaging The Trithene TS 7010 resin is a low-density polyethylene (LDPE) with a high molecular weight, excellent processability, and good mechanical properties. The incorporated additives package warrants th.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ISO 527-3 |
Polimeri Europa Clearflex® CL B0 Very Low Density Polyethylene Clearflex CL B0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin has a high stretchability and a good cling effect.Main Applications: C.. |
|||
Film Tensile Strength at Break, TD | >= 20.0 MPa | >= 2900 psi | ASTM D882 |
Huntsman Rexell® V8801 Cast Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ASTM D882 |
ExxonMobil Escorene® LD-138 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin offering good clarity, toughness, and stiffness. Blown film made from this resin has good machinability in bag equipment a.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ASTM D882 |
LyondellBasell Petrothene® M2520FN Low Density Polyethylene ApplicationsPETROTHENE M 2520 is a film grade resin that exhibits excellent optics, good gloss and good bubble stability. A typical application for this resin is high clarity packaging. Regulatory.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ASTM D882 |
LyondellBasell Petrothene® NA443023 Blown Low Density Polyethylene ApplicationsPETROTHENE NA 443 is a series of low density/EVA copolymer resins for high impact/high clarity packaging applications. NA 443 exhibits excellent processability and good balance of optic.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ISO R527-1 |
Iran Petrochemical (PCC) 2102TX00 Low Density Polyethylene LDPE 2102TX00 GP filmIt is used in wide range of widths and thicknesses e.g. for punches, bags, liners and lamination film.Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ISO R527-1 |
Iran Petrochemical (PCC) 2602TH00 Low Density Polyethylene LDPE 2602TH00 high clarity film Applications: film, underblankets and films for medical applications.Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ISO 527-3 |
Borealis FA6220 Low Density Polyethylene FA6220 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant. This grade is developed for the production of thin blown films. Applications: shrink film, pouches, general packagin.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ISO 527-3 |
Borealis FA6224 Low Density Polyethylene FA6224 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed for the production of thin blown f.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ISO 527-3 |
Borealis Himod™ FT6274 LDPE for Film Himod FT6274 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ISO 527-3 |
Borealis Himod™ FT7293 LDPE for Film Himod FT7293 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ASTM D882 |
Westlake Mxsite LC78104 Polyethylene Mxsite LC78104 polyethylene is recommended for the skin layers of cast stretch film. It will provide a very aggressive cling force in both a stretched and unstretched condition. The excellent cling .. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ASTM D882 |
Chevron Phillips MarFlex® 7109M LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ASTM D882 |
ExxonMobil LD 143.26 High Clarity Packaging Film Resin Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ASTM D882 |
ExxonMobil LDPE LD 143.26 Low Density Polyethylene Resin Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ASTM D882 |
ExxonMobil Optema® TC-114 Blown Ethylene Methyl Acrylate Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown film applications. It produces a soft, elast.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | |
Dow LDPE 681I Low Density Polyethylene, Liner Film Grade DOW LDPE 681I resin is a barefoot general purpose medium duty liner film resin for packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact appl.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ASTM-D882 |
Braskem F 7018 LDPE Extrusion Coating Polyethylene LDPE F 7018 is a low-density polyethylene and has excellent processability and sealability at low temperatures. It does not contain additives. Its applications include: extrusion coating; and injec.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ASTM D882 |
Braskem F0421D Blown Film Extrusion Low Density Polyethylene Shrink films; Automatic packaging of liquid products (FFS).Additives: Antiblock, DInformation provided by Braskem. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ASTM-D882 |
Braskem F2022/0 LDPE Cast Film Extrusion Polyethylene LDPE F2022/0 has excellent sealing characteristics and optical properties with well balanced mechanical properties. Its applications include: general purpose which require no additives; shrink film.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ASTM-D882 |
Braskem F2523 LDPE Blown Film Extrusion Polyethylene LDPE F2523 is a low-density polyethylene. It has good sealing characteristics, optical, and mechanical properties. It contains antiblock and slip additives. Its applications include general purpose .. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ASTM-D882 |
Braskem F7018 LDPE Injection Molding Polyethylene F7018 is a low-density polyethylene with excellent processability and sealability at low temperatures. It does not contain additives. Its applications include: extrusion coating, injection molding .. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ASTM-D882 |
Braskem LBH0120PBS LLDPE Blown Film Extrusion Polyethylene Copolymer LBH0120BPS is a LLDPE Hexene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties as well as s.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ASTM-D882 |
Braskem LF320 LLDPE Cast Film Extrusion Polyethylene Copolymer LF320 is a linear low-density polyethylene, copolymer of butene-1, produced by the gas phase process. It was developed for cast film extrusion. Films obtained with this product show a good processin.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ASTM D882 |
Braskem EB 853 LDPE Cast Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Films for absorbents and diapers (with HDPE and LLDPE); general purpose. Information provi.. |
|||
Film Tensile Strength at Break, TD | 20.0 - 63.6 MPa | 2900 - 9230 psi | Average value: 36.9 MPa Grade Count:11 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ISO 527-3 |
Total LDPE 1022 FN 24 Low Density Polyethylene - Blown Film LDPE 1022 FN 24 is a low density polyethylene made by a high pressure process without antioxidant.LDPE 1022 FN 24 is suited to many applications in the field of consumer, industrial, food or hygiene.. |
|||
Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ASTM D882 |
Braskem F2523 Blown Film Extrusion Low Density Polyethylene Automatic packaging for several products; High transparency films.Additives: Antiblock, DInformation provided by Braskem. |