Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem FG31 LLDPE Blown Film Extrusion Polyethylene Copolymer

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Butene, Film
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem FG31 LLDPE Blown Film Extrusion Polyethylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FG31 is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process. It was developed for blown film extrusion in blends with polyethylene. Films obtained with this product show excellent mechanical properties. FG31 contains antioxidant additives. Its applications include: stretch films, heavy-duty bags, liners, and LDPE and HDPE blends and packages for general use. FG31 resin can be processed with polyethylene on conventional extruders with a maximum ratio of 30%. The best results are obtained with polyethylene resins of low melt index. The recommended temperature profile for blends with LDPE is slightly higher than those ones for the conventional LDPE (10 to 20ºC).
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM-D792
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 930 %
930 %
ASTM-D882
Film Elongation at Break, TD 1280 %
1280 %
ASTM-D882
Elmendorf Tear Strength MD 120 g
120 g
ASTM-D1922
Elmendorf Tear Strength TD 400 g
400 g
ASTM-D1922
Elmendorf Tear Strength, MD 4.80 g/micron
122 g/mil
ASTM-D1922
Elmendorf Tear Strength, TD 16.0 g/micron
406 g/mil
ASTM-D1922
Dart Drop 3.20 g/micron
81.3 g/mil
ASTM-D1709
Dart Drop Test 80.0 g
0.176 lb
ASTM-D1709
Film Tensile Strength at Break, MD 40.0 MPa
5800 psi
ASTM-D882
Film Tensile Strength at Break, TD 30.0 MPa
4350 psi
ASTM-D882
1% Secant Modulus, MD 160 MPa
23200 psi
ASTM-D882
1% Secant Modulus, TD 180 MPa
26100 psi
ASTM-D882
Optical Properties Metric English Comments
Haze 11 %
11 %
ASTM-D1003
Gloss 107 %
107 %
Angle 60°; ASTM-D2457