Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Buckeye Polymers BP ABS 3726 E ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Extruded
Manufacturer Buckeye Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP ABS 3726 E ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ExtrusionABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of processing and outstanding surface appearance.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
Melt Flow 3.0 g/10 min
3.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 34.5 MPa
5000 psi
ASTM D638
Elongation at Break 70 %
70 %
ASTM D638
Flexural Modulus 1.80 GPa
261 ksi
ASTM D790
Izod Impact, Notched 3.60 J/cm
6.74 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C
210 °F
ASTM D648
Processing Properties Metric English Comments
Drying Temperature 80.0 °C
176 °F
in air circulating oven recommended
Dry Time 3 - 4 hour
3 - 4 hour