Buckeye Polymers BP FLEX D5518 R 848 Thermoplastic Polyolefin

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Buckeye Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP FLEX D5518 R 848 Thermoplastic Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resistanceGood UV resistanceLow densityWide service range from -20°C to 120°CAppearance: Black or NaturalForms: Strand or Gala cutProcessing Method: Injection MoldingInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.012 - 0.015 cm/cm
0.012 - 0.015 in/in
ASTM D955
Melt Flow 15 - 19 g/10 min
15 - 19 g/10 min
ASTM D1238
Ash 2.0 - 7.0 %
2.0 - 7.0 %
ASTM D5630
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 12.0 MPa
>= 1740 psi
ASTM D638
Flexural Modulus 0.4699 - 0.94975 GPa
68.15 - 137.75 ksi
ASTM D790
Izod Impact, Notched >= 0.534 J/cm

@Temperature -30.0 °C
>= 1.00 ft-lb/in

@Temperature -22.0 °F
ASTM D256
>= 2.14 J/cm

@Temperature 23.0 °C
>= 4.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Gardner Impact >= 190 J
>= 140 ft-lb
ASTM D5420