Buckeye Polymers BP RPP 1209 GR BLK Polypropylene, 12% Glass Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Glass Fiber Filler
Manufacturer Buckeye Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP RPP 1209 GR BLK Polypropylene, 12% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Information: 12% glass reinforced polypropyleneProduct Features:Offers improved flex modulus while maintaining a low specific gravity propertyOffers improved heat stability and scratch and mar resistanceAppearance: BlkForms: Strand Cut PelletsInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.970 - 0.990 g/cc
0.970 - 0.990 g/cc
ASTM D792
Melt Flow 8.0 - 14 g/10 min
8.0 - 14 g/10 min
ASTM D1238
Ash 10 - 14 %
10 - 14 %
ASTM D5630
Mechanical Properties Metric English Comments
Flexural Modulus >= 2.59 GPa
>= 375 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256