Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 9.0 - 14 g/10 min | 9.0 - 14 g/10 min | ASTM D1238 |
S&E Specialty Polymers GPP1001HFNH-2-AT(18) PP Application: Non-halogen flame retardant UL-94 V0 polypropylene compound.Information provided by S&E Specialty Polymers |
|||
Melt Flow | 3.0 - 14 g/10 min | 3.0 - 14 g/10 min | ASTM D1238 |
Polymer Resources ABS-GP1-[color]-3 ABS, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 3.0 - 14 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.0 - 14 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Melt Flow | 3.0 - 14 g/10 min @Load 5.00 kg, Temperature 250 °C |
3.0 - 14 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources PC/ABS-G10 General Purpose PC/ABS Alloy, 10% Glass Filled PC/ABS Alloy, General Purpose, 10% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Melt Flow | 3.0 - 14 g/10 min @Load 5.00 kg, Temperature 250 °C |
3.0 - 14 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Melt Flow | 3.0 - 14 g/10 min @Load 5.00 kg, Temperature 250 °C |
3.0 - 14 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources PC/ABS-GP1 General Purpose PC/ABS Alloy PC/ABS Alloy, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Re.. |
|||
Melt Flow | 3.0 - 14 g/10 min @Load 5.00 kg, Temperature 250 °C |
3.0 - 14 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources PC/ABS-GP1-[color]-EP General Purpose PC/ABS Alloy, Electroplating Grade PC/ABS Alloy, General Purpose, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p.. |
|||
Melt Flow | 3.0 - 14 g/10 min @Load 5.00 kg, Temperature 250 °C |
3.0 - 14 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources PC/ABS-GP1-[color]-LG General Purpose PC/ABS Alloy, Low Gloss Grade PC/ABS Alloy, General Purpose, Low Gloss GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid.. |
|||
Melt Flow | 10 - 14 g/10 min @Load 2.16 kg, Temperature 230 °C |
10 - 14 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 1552N (YF39S) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Melt Flow | 10 - 14 g/10 min | 10 - 14 g/10 min | 230/2.16 (typical); ASTM D1238 |
Fiberfil® PP-61/VO/NH Polypropylene Copolymer, Flame Retardant, non-halogenated, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Melt Flow | 10 - 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
10 - 14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem PCD 0810 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Melt Flow | 11 - 14 g/10 min @Load 2.16 kg, Temperature 235 °C |
11 - 14 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238 |
Gromax PBT 1100-211H Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melt Flow | 6.0 - 14 g/10 min @Load 5.00 kg, Temperature 200 °C |
6.0 - 14 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Kraton® D4271 J (O/E SBS) Branched Block Copolymer Description: Kraton D4271 J is an oil-extended branched block copolymer based on styrene and butadiene, with bound styrene of 45% mass. It is supplied from Japan in the physical forms identified in .. |
|||
Melt Flow | 10 - 14 g/10 min | 10 - 14 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 6221 BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 10 - 14 g/10 min | 10 - 14 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 6221 C BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 10 - 14 g/10 min | 10 - 14 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 6221 C NAT The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 10 - 14 g/10 min @Load 2.16 kg, Temperature 230 °C |
10 - 14 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Samyang Triel® 5552EM Thermoplastics Polyetherester Elastomer, Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5552EM is an extrusion grade.Information provided by Samyang. |
|||
Melt Flow | 9.0 - 14 g/10 min @Temperature 230 °C |
9.0 - 14 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ FPP 2121UV-M-31 Black Filled Polypropylene Homopolymer DescriptionPolyfort® FPP 2121UV-M-31 is a 30% black filled polypropylene homopolymer. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman... |
|||
Melt Flow | 9.0 - 14 g/10 min @Load 2.16 kg, Temperature 280 °C |
9.0 - 14 g/10 min @Load 4.76 lb, Temperature 536 °F |
Z-011A |
Zeon Chemicals Zeonex® 330R Cyclo-Olefin Polymer Zeonex®330R has a lower birefringence than other Zeonex® products. This grade can satisfy market demands in the optical area where low birefringence and high dimensional stability in precision opt.. |
|||
Melt Flow | 9.0 - 14 g/10 min @Temperature 230 °C |
9.0 - 14 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ FPP 2121UV-M-31 Black Filled Polypropylene Homopolymer DescriptionPolyfort® FPP 2121UV-M-31 is a 30% black filled polypropylene homopolymer. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman... |
|||
Melt Flow | 9.0 - 14 g/10 min @Temperature 230 °C |
9.0 - 14 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ FPP 2121UV-M-31 Black Filled Polypropylene Homopolymer DescriptionPolyfort® FPP 2121UV-M-31 is a 30% black filled polypropylene homopolymer. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman... |
|||
Melt Flow | 9.0 - 14 g/10 min @Temperature 230 °C |
9.0 - 14 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ FPP 2121UV-M-31 Black Filled Polypropylene Homopolymer DescriptionPolyfort® FPP 2121UV-M-31 is a 30% black filled polypropylene homopolymer. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman... |
|||
Melt Flow | 10 - 14 g/10 min | 10 - 14 g/10 min | ASTM D1238 |
Buckeye Polymers BP FLEX D5512 RU BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Melt Flow | 10 - 14 g/10 min | 10 - 14 g/10 min | ASTM D1238 |
Buckeye Polymers BP FLEX D6512 BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Melt Flow | 8.0 - 14 g/10 min | 8.0 - 14 g/10 min | ASTM D1238 |
Buckeye Polymers BP PPC 0212 BLK Polypropylene Copolymer Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis.. |
|||
Melt Flow | 6.0 - 14 g/10 min @Load 21.6 kg, Temperature 232 °C |
6.0 - 14 g/10 min @Load 47.6 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR® 461 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan.. |
|||
Melt Flow | 10 - 14 g/10 min | 10 - 14 g/10 min | ASTM D1238 |
Buckeye Polymers BP RPP 2010 T NAT Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |
|||
Melt Flow | 6.0 - 14 g/10 min @Load 21.6 kg, Temperature 232 °C |
6.0 - 14 g/10 min @Load 47.6 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Melt Flow | 4.0 - 14 g/10 min @Load 12.5 kg, Temperature 232 °C |
4.0 - 14 g/10 min @Load 27.6 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Melt Flow | 2.0 - 14 g/10 min @Load 3.80 kg, Temperature 232 °C |
2.0 - 14 g/10 min @Load 8.38 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR® 2501-20 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. Very flexible, very soluble. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low p.. |