Buckeye Polymers BP RPP 3012 C NAT Polypropylene, Calcium Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
Manufacturer Buckeye Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP RPP 3012 C NAT Polypropylene, Calcium Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Information: Calcium Carbonate Filled PP Grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. Our BP RPP C series product line ranges from 10-50% in filler levels. These materials can be customized through the addition of UV packages, custom matching, and processing additives.Product Features:Can be UV stabilized for increased resistanceIndustrial, outdoor furniture, and window trim.Processing Method: Injection MouldingInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Melt Flow 6.0 - 12 g/10 min
6.0 - 12 g/10 min
ASTM D1238
Ash 27 - 33 %
27 - 33 %
ASTM D5630