Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bulk Molding Compounds BMC T44 High Strength Mineral Filled Molding Compound

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester, Mineral Filled
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC T44 High Strength Mineral Filled Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC T44 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displacing engineered phenolic materials in automotive slip-ring as well as commutator applications. Other uses are in welder tips and handles as well as structural parts.Information provided by Bulk Molding Compounds, Inc.
Physical Properties Metric English Comments
Density 1.59 - 1.79 g/cc
0.0574 - 0.0647 lb/in³
Molded
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
0.0015 - 0.0025 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 30 - 40
30 - 40
Tensile Strength 65.5 - 79.3 MPa
9500 - 11500 psi
Flexural Strength 152 - 179 MPa
22000 - 26000 psi
Flexural Modulus 8.96 - 10.3 GPa
1300 - 1500 ksi
Compressive Strength 117 - 145 MPa
17000 - 21000 psi
Izod Impact, Notched 7.26 - 8.33 J/cm
13.6 - 15.6 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 218 - 260 °C
425 - 500 °F
Flammability, UL94 HB
HB
This product is not currently UL listed.
Electrical Properties Metric English Comments
Dielectric Strength 13.6 - 15.6 kV/mm
345 - 395 kV/in
short time
Arc Resistance 188 sec
188 sec
Processing Properties Metric English Comments
Processing Temperature 143 - 171 °C
290 - 340 °F
Users viewing this material also viewed the following: