Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.59 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183/A
Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in water-c..
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
PTS Lucet® GC-225 25% Glass Reinforced Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183
Celanese Hostaform® C 27021 GV3/30 POM, 30% Glass Reinforced  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade with high flow, with 30 % glass spheres reinforcedInformation provided by Celanese
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183
LATI LATAN 13 G/303 30% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)  (discontinued **)
Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea..
Density 1.59 - 1.60 g/cc
0.0574 - 0.0578 lb/in³
Average value: 1.59 g/cc Grade Count:5
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E..
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183
DSM Akulon® S224-KMV7 Nylon 66-35% Mineral Reinforced (European and Asian Grade) (Dry)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Density 1.59 - 1.63 g/cc
0.0574 - 0.0589 lb/in³
ISO R 1184
Fainplast Compounds RE 241 Rigid PVC, Extrusion
Various profiles
Density 1.59 g/cc
0.0574 lb/in³
K3425A; ASTM D1475-85
Lord Adhesives Aeroglaze® K3425 Sandable Primer/Surfacer
For application on epoxy graphite or other plastic substrates or over a suitable primer on metal.Limitations - Aeroglaze® K3425 primer/surfacer contains no inhibiting pigments and is not suitable..
Density 1.59 g/cc
0.0574 lb/in³
LATI Latilub 66-01M G/50 PA66, 50% Glass Fiber Reinforced, Molybdenum disulphide Filled
Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
Density 1.59 g/cc
0.0574 lb/in³
LATI Latishield 85-08A G/20 PES, Steel/Glass Fibers
EMI shielding product based on Polyether Sulfone (PES). Steel fibers. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati ..
Density 1.59 g/cc
0.0574 lb/in³
Dry; ASTM D792
Solvay Specialty Polymers Omnix® 4050 Polyamide, High Performance (HPPA) (Conditioned)
Omnix® 4050 is a 50% glass-fiber reinforced, high-performance polyamide (HPPA). It is particularly suited for replacing die-cast metal in a variety of mechanical applications and components used ..
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
Solvay Specialty Polymers Omnix® 4050 Polyamide, High Performance (HPPA) (Dry)
Omnix® 4050 is a 50% glass-fiber reinforced, high-performance polyamide (HPPA). It is particularly suited for replacing die-cast metal in a variety of mechanical applications and components used ..
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
Techmer ES HiFill® PP 0159 B Polypropylene
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc.
Density 1.59 g/cc
0.0574 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp OK006 PPS - Linear
LNP* Thermocomp* OK006 is based on a Linear Polyphenylene Sulfide (PPS) containing Talc.This data was supplied by SABIC-IP for the Americas region.
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
Plenco 00732 Melamine-Phenolic, Granular, Transfer Molded
PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007..
Density 1.59 g/cc
0.0574 lb/in³
DIN 53479
Polyram RamSter PF320G4 PBT, 20% Glass Fiber, Flame Retardant
20% Glass fiber reinforced, flame retardant PBT for injection molding applicationsInformation provided by Polyram Ram On Ind.
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
Toyobo VYLOPET® EMC310TU Injection Molding Polyester Resin, Warpageless, High cycles
Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesWarpagelessInformation provided by Toyobo.
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183
Polyplastics FR-PET® C9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
Information provided by PolyPlastics.
Density 1.59 g/cc
0.0574 lb/in³
Trelleborg Emerson & Cuming Stycast® S5225 Two-Component Easy Mix Ratio Encapsulant
Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, ..
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183
EMS-Grivory Grivory® G4V-5H black 9915 PA*-GF50
Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio..
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183
EMS-Grivory Grivory® HTV-45H1 black 9205 PA6T/6I-GF45
Product description: Grivory HTV-45H1 black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation a..
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183
EMS-Grivory Grivory® XE 5107 (GVL-5H V0) PA*-GF50
Product description: Grivory XE 5107 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf..
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183
Barlog Plastics KEBAFORM C 906 GB POM Copolymer, 30% glass bead reinforced
POM-GB30Information provided by BARLOG plastics GmbH.
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Conditioned, 50% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Density 1.59 g/cc
0.0574 lb/in³
A. Schulman ComAlloy Voloy® 411 Mineral Reinforced, PBT Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.25% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183
Celanese IMPET 830R PET, 35% Mineral / Glass Reinforced
Impet 830R is a 35% glass/mineral reinforced injection moldable polyester made with recycled PET. It provides an excellent combination of strength, stiffness, warp resistance, and high temperature c..
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
Plaslok 5303 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5303 is a two-stage, mineral and floc..
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183
Celanese Hostaform® C 27021 GV3/30 POM, 30% Glass Reinforced
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183
SABIC Innovative Plastics LNP VERTON RX06097 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RX06097 is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, UV-Stabilized.
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
Plenco 50030 PET, Pellet, Injection Molded, Natural Color  (discontinued **)
PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup..
Copyright © lookpolymers.com All Rights Reserved