CMT Materials HYTAC® WFT High Temperature, Ultra-Smooth PTFE Impregnated

Category Polymer , Thermoset , Epoxy
Manufacturer CMT Materials
Trade Name HYTAC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMT Materials HYTAC® WFT High Temperature, Ultra-Smooth PTFE Impregnated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HYTAC-WFT combines the higher temperature, smooth surface properties of HYTAC-WF with PTFE impregnation for low stick surface capability and excellent material distribution. The result is a syntactic plug assist material with a service temperature of 4250F that may be polished to an ultra-smooth surface.The intended uses of HYTAC-WFT are for difficult sheet sticking problems or in situations where an extremely smooth surface is critical to part quality. As with other syntactic materials, HYTAC-WFT offers the following advantages: Low thermal conductivity and specific heatDimensionally stableExcellent temperature resistanceLightweight Easily machined Variety of Shapes and Sizes: The material is provided in standard sized rods or sheets, but may be custom molded to meet the specific needs. Applications: HYTAC-WFT machines and polishes to an ultra-smooth finish. Recommended for use with CPET, EVOH, LDPE, PC, PMMA, PS and RPET Information Provided by CMT Materials, Inc.
Physical Properties Metric English Comments
Density 0.801 - 0.961 g/cc
0.0289 - 0.0347 lb/in³
Mechanical Properties Metric English Comments
Flexural Toughness 0.0310 MPa
4.50 psi
ASTM D790
Compressive Strength 121 MPa
17500 psi
Compressive Modulus 2.24 GPa
325 ksi
Thermal Properties Metric English Comments
CTE, linear 36.7 µm/m-°C
20.4 µin/in-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 218 °C
425 °F
Descriptive Properties Value Comments
Color Light Green