Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 218 °C | 425 °F | |
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i.. |
|||
Maximum Service Temperature, Air | 218 °C | 425 °F | Long Term |
Quadrant EPP Techtron® 1000 PPS Extruded Polyphenylene Sulfide (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 218 °C | 425 °F | |
Quantum PPS Information provided by Quantum Advanced Engineering Plastics |
|||
Maximum Service Temperature, Air | 218 °C | 425 °F | |
Glastic GLASTHERM S Insulation Sheet Glastherm Grade S is a general purpose insulation sheet with an economical combination of thermal and physical properties. Not recommended for processes where the continuous operating temperature e.. |
|||
Maximum Service Temperature, Air | 218 °C | 425 °F | |
Greene Tweed CHEMRAZ® 528 Perfluoroelastomer Chemraz® 528 works well in a wide variety of biotechnology and medical device applications where ling-term seal reliability is required. This seal material offers excellent performance in static.. |
|||
Maximum Service Temperature, Air | 218 °C | 425 °F | ASTM D1329 |
Seals Eastern 7182D Fluorocarbon-Elastomer Formulated AFLAS® high-temperature "sour" oil & gas service. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |
|||
Maximum Service Temperature, Air | 218 °C | 425 °F | ASTM D1329 |
Seals Eastern 7182X Fluorocarbon-Elastomer Formulated AFLAS®. Ultra-low compressive stress relaxation for alkaline, high-temperature service.Information provided by Seals Eastern, Inc. |
|||
Maximum Service Temperature, Air | 218 °C | 425 °F | Short Term |
Saint-Gobain Rulon® II Bearing/Seal PTFE An injection moldable bearing material that possesses excellent chemical and wear resistance. Rulon II is available in injection molded finished parts only. Excellent friction and wear properties al.. |
|||
Maximum Service Temperature, Air | 218 °C | 425 °F | ASTM D1329 |
Seals Eastern 7182B Fluorocarbon-Elastomer Formulated AFLAS® high-temperature, high-pressure "sour" oil & gas service. ED resistant. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |
|||
Maximum Service Temperature, Air | 218 °C | 425 °F | |
Master Bond Supreme 33 High Temperature Resistant, Structural Adhesive Description: Master Bond Polymer System Supreme 33 is a unique, room temperature curing, toughened epoxy adhesive/sealant, offering high temperature resistance. This innovative system offers high bo.. |
|||
Maximum Service Temperature, Air | 218 °C | 425 °F | |
Master Bond Supreme 33CLV Two Component, Room Temperature Curing Toughened Epoxy Master Bond Polymer System Supreme 33CLV is a special, room temperature curing, toughened epoxy adhesive/sealant, featuring exceptionally high temperature resistance. This innovative system has outs.. |
|||
Maximum Service Temperature, Air | 218 °C | 425 °F | |
CMT Materials HYTAC® WFT High Temperature, Ultra-Smooth PTFE Impregnated HYTAC-WFT combines the higher temperature, smooth surface properties of HYTAC-WF with PTFE impregnation for low stick surface capability and excellent material distribution. The result is a syntact.. |