Material Notes:
ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and thermal conductivity and ductility.ELKALOY® D120 material is recommended for heavy-duty butt or flash welding jaws, clamps and dies. It is also used for machine parts to resist heavy pressure and extreme wear. It is a superior material as a guide bushing for automatic arc welders, heavy-duty bearings slides and gibbs when used in contact with steel.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 7.50 g/cc
0.271 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 95
95
Tensile Strength, Ultimate 586 MPa
85000 psi
Tensile Strength, Yield 276 MPa
40000 psi
Elongation at Break 4.0 %
4.0 %
Reduction of Area 3.0 %
3.0 %
Modulus of Elasticity 97.0 GPa
14100 ksi
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Temperature 100 °C
10.0 µin/in-°F

@Temperature 212 °F
Thermal Conductivity 71.0 W/m-K
493 BTU-in/hr-ft²-°F
Melting Point 1025 - 1060 °C
1877 - 1940 °F
Solidus 1025 °C
1877 °F
Liquidus 1060 °C
1940 °F
Component Elements Properties Metric English Comments
Aluminum, Al 11.6 %
11.6 %
Beryllium, Be 0.50 %
0.50 %
Co + Ni 1.5 - 2.55 %
1.5 - 2.55 %
Copper, Cu 81.45 - 82.5 %
81.45 - 82.5 %
Iron, Fe 3.9 %
3.9 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000172 ohm-cm
0.0000172 ohm-cm
10 % IACS