Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 276 MPa | 40000 psi | |
Pacific Sintered Materials F-244-S High Carbon Steel Powdered Metal Applications:Highly stressed mechanical componentsGood hardenabilityEquivalent MPIF Specification: F-0008-35All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
Pacific Sintered Materials FCC-221-P Copper Steel Powdered Metal Applications:Medium strength mechanical componentsEquivalent MPIF Specification: FC-0205-35All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
Pacific Sintered Materials FN-251-S Invar Powdered Metal Coefficient of thermal expansion equal to glass.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
Pacific Sintered Materials FN-262-S High Strength Nickel Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability.Equivalent MPIF Specification: FN-0405-35All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
Pacific Sintered Materials SS-316-RD 316L Stainless Steel Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.Equivalent MPIF Specification: SS-316-40All information provided by Pacific Sin.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 %, Temperature 538 °C |
40000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Ultimet® alloy, 12.7-50.8 mm bar Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 276 - 483 MPa | 40000 - 70100 psi | |
Materion Beryllium Nickel Strip - Alloy 360 Annealed Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): .. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 CF40 HS 40% Carbon Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | ASTM D638 |
Techmer ES HiFill® PEEK CF40 HF 40% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Europe-Africa-Middle East) LNP VERTON* RV00AES is a compound based on PA 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Verton RV00AESM PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AESM is a compound based on PA66 resin containing Long Glass Fiber. Added features include: Easy Moldin, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RV00AESS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AESS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, Heat Stabilized. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RV00AEX5 PA6.6 (Europe-Africa-Middle East) LNP* VERTON* Is a compound based on PA66 resin containing Long Glass Fiber. Added features include: Easy Molding, Heat Stabilized. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
Universal Wire Works Inconel 62 (AMS 5679) Nickel Alloy Filler Metal Inconel Filler Metal 62 is a nickel chromium alloy designed for welding nickel base alloy 600 in up to 2" thicknesses using the gas tungsten arc, gas metal arc and submerged arc processes. Filler Me.. |
|||
Tensile Strength, Yield | 276 - 345 MPa | 40000 - 50000 psi | 0.2% offset |
Eagle Brass 151 ZHC® COPPER, 1/2 Hard Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Tensile Strength, Yield | 276 - 379 MPa | 40000 - 55000 psi | 0.2% offset |
Eagle Brass 519 Phosphor Bronzes 6%, 1/4 Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
Crucible Steel 348 Chromium-Nickel Steel Crucible 348 is a non-hardenable austenitic chromium-nickel steel which are particularly adaptable for use at temperatures between 800 and 1650°F. This grade is non-magnetic in the annealed conditi.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition A AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
AK Steel 321 Austenitic Stainless steel AK Steel 321 is a stabilized austenitic stainless steel similar to Type 304 but with a titanium addition. This titanium addition reduces or prevents carbide precipitation during welding and in 427 .. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 %, Temperature 93.0 °C |
40000 psi @Strain 0.200 %, Temperature 199 °F |
|
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
Carpenter 20-Mo6® Stainless Steel, Strip Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
Annealed |
AK Steel 410S Ferritic Stainless steel AK Steel 410S Stainless Steel is a non-hardening modification of Type 410. A small titanium addition minimizes austenite formation at high temperatures, thereby restricting the alloy's ability to h.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
Carpenter Invar 36® Alloy, Annealed Bars and Strip Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
ATI Allvac® Grade 7 UNS R52400 Titanium Alloy Uses: Industrial components, CPI equipment, heat exchangers, pressure vessels, fittings, tubings.Property values are for samples in the metallurgical condition: 1300°F anneal.Information provided b.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® 600 Nickel Superalloy, Heat Treatment: 927°C (1700°F) Anneal Data provided by Allvac.Applications: Aircraft engines, nuclear reactor applications, chemical process equipment, high temperature fixtures. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® H-X Nickel Superalloy, Heat Treatment: 1177°C (2150°F) Anneal Data provided by Allvac.Applications: Afterburner components, combustion chamber liners, nozzles, vanes, rings, turbine exhaust weldments, structural parts. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
ATI Allvac® 40, Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal Data provided by Allvac.Applications: Airframe components, cryogenic vessels, heat exchangers, CPI equipment, condenser tubing, pickling baskets. |
|||
Tensile Strength, Yield | 276 - 345 MPa @Strain 0.200 % |
40000 - 50000 psi @Strain 0.200 % |
|
AK Steel 436L ULTRA FORM® Ferritic Stainless Steel AK Steel’s 436L ULTRA FORM® is a ferritic grade of stainless steel that outperforms Type 409 in oxidation resistance and corrosion testing. The addition of molybdenum enhances pitting resistance w.. |
|||
Tensile Strength, Yield | 276 - 331 MPa @Strain 0.200 %, Thickness 1.02 - 1.78 mm |
40000 - 48000 psi @Strain 0.200 %, Thickness 0.0402 - 0.0701 in |
|
AK Steel 439 LT Ferritic Stainless steel AK Steel 439 LT has oxidation and corrosion resistance comparable to Type 439 stainless steel. This alloy also has optimum formability that is reproducible coil after coil and heat after heat. Thi.. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
Mueller Ecostream™ C36500 Uninhibited Leaded Muntz Metal As one of the lower lead alloys offered in the EcoStream™ family of products, Mueller Brass Company’s C36500 alloy provides a viable alternative to those manufacturers who are manufacturing produc.. |